07   Thermowood Species   ·   American South timber basket

The hardest softwood in our range

Thermo SYP

Pinus taeda — thermally modified at 212°C

Southern Yellow Pine from the southeastern United States — the densest, hardest commercial softwood we modify. Strong latewood bands give the board its signature high-contrast grain striping after the kiln darkens it.

Raw density

570kg/m³densest softwood we stock

Denser than Scots Pine (~500) and Radiata (~500). SYP's heavy latewood bands are why American builders frame with it.

Botanical

Pinus taeda

Density

480–510 kg/m³

Durability

EN 350 Class 2

Service life

20+ yr Indian climate

Chemicals

None — heat & steam

Species overview

The American workhorse, baked stable.

Pinus taeda — loblolly, the backbone of the Southern Yellow Pine group — comes from the managed timber basket of the southeastern United States, one of the largest working forest systems in the world. Boards arrive kiln-dried to 10–12% moisture at our Gandhidham facility.

SYP is the hardest and densest of the commercial softwoods — raw Brinell around 2.2 N/mm² against Scots Pine's 1.9. Its strong latewood bands produce a bold striped grain that darkens dramatically through the ThermoWood-D cycle. Durability moves from class 4–5 to class 2; the bold grain stays.

Hardness among softwoods

#1 in range

Brinell ~2.2 N/mm² raw — the hardest softwood we modify, above Scots Pine and Radiata.

Grain contrast

High

Strong latewood bands — the boldest stripe pattern of our softwoods. Reads stronger after the kiln darkens it.

Full specification

Thermo SYP — raw vs modified.

Every value below is sourced from an independently published technical standard or the ThermoWood Association technical handbook. Nothing is estimated or marketing-derived.

Values double-verified
Property
Raw Thermo SYP
After Thermowood-D
Source
Equilibrium moisture content
~12%
4–6%
ThermoWood Handbook, Section 2.2
Dimensional movement
Typical dense softwood
50–60% less
ThermoWood Handbook; ISO 21887
Density @ 12% MC
~570 kg/m³
480–510 kg/m³
USDA FPL; The Wood Database
EN 350 natural durability (heartwood)
Class 4–5 — slightly durable
Class 2 — durable
EN 350:2016; CEN/TS 15679
Service life, Use Class 3
5–10 years
25–30 yr Nordic20+ yr Indian climate
ThermoWood Assn; EN 335
Brinell hardness
~2.2 N/mm²
1.9–2.1 N/mm²
EN 1534:2020; USDA FPL
Thermal conductivity
~0.13 W/mK
0.09–0.11 W/mK
ThermoWood Handbook
Fire reaction (untreated)
Class D-s2,d0
Class D-s2,d0
EN 13501-1; FR-coated on request
Colour
Yellow with amber latewood
Striped honey-to-umber throughout
Caramelised pyrolysis, through thickness

Primary sources: International ThermoWood® Association technical handbook (Finnish Thermowood Association); USDA Forest Products Laboratory, FPL-GTR-190 Chapter 19; The Wood Database; EN 350:2016; EN 335:2013; EN 13501-1:2018; EN 1534:2020; CEN/TS 15679:2007; ISO 21887. FSC Chain of Custody SCS-COC-006930. Independent test reports available per project on request.

Where it goes

Five applications.

01Decking
02Facade cladding
03Wall panelling
04Ceiling slats
05Pergolas & outdoor structures

Full process explanation on the Thermowood range page. Install specifications issued per project — request technical PDF.

Specify Thermo SYP

See the board before you specify it.

Order free samples, download the technical datasheet, or send us the BOQ. We come back with profile, lead time and pricing. Shipped pan-India from Kaithal.

Product Enquiry

Share your details and our team will get back with samples, sizes & pricing.